Failure Test

Failure Test
FpressviceAA
Plate angle
0°
Cracknone
Lack of fusionnone
Lack of penetrationnone
Solid inclusionnone
PoreØ 0.8 mm
sample · a = 5 mm, weld length 100 mm
01 / 05

Fillet-welded specimen

A single-sided fillet weld on a T-joint; it will be loaded so that the weld root is in tension.

02 / 05

Clamping

The base plate is clamped in a vice; the upright plate is free.

03 / 05

Loading

The press pushes the upright away from the weld; the root opens and stress concentrates in the weld throat.

04 / 05

Fracture

A crack starts at the root and runs through the throat; the weld breaks and the plate folds over.

05 / 05

Examining the fracture face

The fracture surface is examined and measured for porosity, cracks, lack of fusion, lack of penetration and solid inclusions.

It is aimed to ensure that the test samples removed from the welded joints break from the weld metal and examine the broken surfaces. Testing is performed to obtain information about the types, sizes and distributions of internal defects on the fracture surfaces, examples of which are given below.

  • Pores
  • Cracks
  • Melting deficiencies
  • Lack of penetration
  • Solid residues

Photos

Fillet weld broken in the fracture test
Fillet weld broken in the fracture test1 / 1